ASTM A234 WPB & WPC piipfittingen ynklusyf elbows, T-stukken, reducers
Gemyske gearstalling fan ASTM A234 WPB & WPC
Elemint | Ynhâld, % | |
ASTM A234 WPB | ASTM A234 WPC | |
Koalstof [C] | ≤0.30 | ≤0.35 |
Mangaan [Mn] | 0.29-1.06 | 0.29-1.06 |
Fosfor [P] | ≤0.050 | ≤0.050 |
Sulfur [S] | ≤0.058 | ≤0.058 |
Silisium [Si] | ≥0.10 | ≥0.10 |
Chromium [Cr] | ≤0.40 | ≤0.40 |
Molybdeen [Mo] | ≤0.15 | ≤0.15 |
Nikkel [Ni] | ≤0.40 | ≤0.40 |
Koper [Cu] | ≤0.40 | ≤0.40 |
Vanadium [V] | ≤0.08 | ≤0.08 |
*It koalstofekwivalint [CE=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15] moat net grutter wêze as 0,50 en moat rapportearre wurde op MTC.
Mechanyske eigenskippen fan ASTM A234 WPB & WPC
ASTM A234-klassen | Treksterkte, min. | Opbringststerkte, min. | Ferlinging %, min. | |||
ksi | MPa | ksi | MPa | Longitudinaal | Transversaal | |
WPB | 60 | 415 | 35 | 240 | 22 | 14 |
WPC | 70 | 485 | 40 | 275 | 22 | 14 |
*1. WPB- en WPC-piipfittingen makke fan platen moatte in minimale ferlinging fan 17% hawwe.
*2. Behalven as it fereaske is, hoecht de hurdheidswearde net rapportearre te wurden.
Produksje
De ASTM A234 koalstofstiel piipfittings kinne makke wurde fan naadleaze pipen, lassen pipen of platen troch foarmjaanoperaasjes lykas persen, trochboarjen, ekstrudearjen, bûgen, fusielassen, masinearjen, of troch in kombinaasje fan twa of mear fan dizze operaasjes. Alle lassen, ynklusyf lassen yn buisfoarmige produkten wêrfan fittings makke binne, moatte makke wurde yn oerienstimming mei ASME Seksje IX. Nei it lasproses moatte waarmtebehanneling by 595 oant 675 °C en radiografysk ûndersyk útfierd wurde.